Pyrophyl R-1404

Oxide Analysis Formula
K2O 0.20% 0.01
Na2O 0.20% 0.02
TiO2 0.40% 0.03
Al2O3 20.00% 1.00
SiO2 75.60% 6.42
Fe2O3 0.70% 0.02
LOI2.90%
Oxide Weight 495.21
Formula Weight 510.00

Related Information

Links

Materials Pyrophyl
Suppliers RESCO Products
Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

By Tony Hansen