Pyrophyl R-1403

Pyrophyllite

OxideAnalysisFormula
K2O0.20%0.010
Na2O0.20%0.016
TiO20.40%0.024
Al2O321.00%1.000
SiO274.70%6.037
Fe2O30.70%0.021
LOI2.80
Oxide Weight472.11
Formula Weight485.71
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.70
SADR - Sieve Analysis Dry +200 mesh: 12%
PCE - Pyrometric Cone Equivalent 29
BDLB - Bulk Density lbs/cu. ft. (Packed) 60

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications.

Pyrophyl is a high melting material and is used to reduce hot load deformation and improve volume stability in refractories.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pyrophyl R-1403" descrip="Pyrophyllite" searchkey="" loi="2.80" casnumber="12269-78-2"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="74.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="2.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved