Pyrophyl

Pyrophyllite

OxideAnalysisFormula
K2O0.20%0.010
Na2O0.20%0.015
TiO20.40%0.023
Al2O322.30%1.000
SiO273.30%5.579
Fe2O30.70%0.020
LOI2.80
Oxide Weight444.13
Formula Weight456.93
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.7-2.75
SADR - Sieve Analysis Dry +200 mesh: 1-12%
PCE - Pyrometric Cone Equivalent 26-29
BDLB - Bulk Density lbs/cu. ft. (Packed) 55-70

The PYROPHYL group of mineral products consists of milled co-products of the Andafrac series and various milled combinations of the Pyrofrac and Andafrac series. The broad range of alumina contents allows for both whiteware and refractory applications.

Pyrophyl is a high melting material and is used to reduce hot load deformation and improve volume stability in refractories. It is used in foundry mold and core wash formulations, technical ceramics, structural clay coatings, art pottery.

This material is dry milled and magnetically separated.

The analysis shown here is an average.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pyrophyl" descrip="Pyrophyllite" searchkey="" loi="0.00" casnumber="12269-78-2"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="22.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="73.300" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="2.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved