Pyrofrac 2023

OxideAnalysisFormula
K2O0.20%0.010
Na2O0.20%0.016
TiO20.40%0.024
Al2O321.00%1.000
SiO272.40%5.851
Fe2O31.00%0.030
Cl4.80
Oxide Weight462.40
Formula Weight485.71
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 2.7
SADR - Sieve Analysis Dry +20 mesh: 10.1 +50 mesh: 59.3 +70 mesh: 13.5 +100 mesh: 8.2 +200 mesh: 7.0 +325 mesh: 1.0
PCE - Pyrometric Cone Equivalent 29
BDLB - Bulk Density lbs/cu. ft. (Packed) 70

Used in structural clay coatings, refractory formulations, whiteware ceramics, art pottery to
increase refractoriness, reduce shrinkage, and widen firing range.
This material is made by crushing & screening of selectively mined andalusite/pyrophyllite/sericite ores
with heavy media separation.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pyrofrac 2023" descrip="" searchkey="" loi="0.00" casnumber="12269-78-2"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="21.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="72.400" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.000" tolerance=""/> </oxides> <volatiles> <volatile symbol="Cl" name="Chlorine Gas" percent="4.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved