PuraFlow AK Ball Clay

Very high plastic buff burning Devon ball clay

Alternate Names: Blue Ball Clay

OxideAnalysisFormula
K2O1.00%0.034
Na2O1.10%0.057
Al2O332.00%1.000
SiO250.00%2.652
Fe2O31.10%0.022
LOI10.00
Oxide Weight271.58
Formula Weight301.75
If this formula is not unified correctly please contact us.

LOI estimated


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PuraFlow AK Ball Clay" descrip="Very high plastic buff burning Devon ball clay" searchkey="Blue Ball Clay" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="32.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.000" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="10.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved