PR#3 D

SANDY TAN-BUFF STONEWARE

OxideAnalysisFormula
CaO0.18%0.020
MgO0.52%0.081
K2O2.60%0.174
Na2O0.11%0.011
P2O50.01%0.000
TiO20.60%0.047
Al2O316.17%1.000
SiO270.98%7.450
Fe2O31.14%0.045
MnO0.01%0.001
LOI6.51
Oxide Weight582.35
Formula Weight622.90
If this formula is not unified correctly please contact us.

Sandy and silty tan burning clean medium fire stoneware mined at Ravenscrag, Sask.

Analysis updated July 97.

539 Ba ppm
37 Sr pmm
23 Y ppm
8 Sc ppm
283 Zr ppm
1 Be ppm
54 V ppm


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PR#3 D" descrip="SANDY TAN-BUFF STONEWARE" searchkey="" loi="6.51" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.180" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.520" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.110" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.170" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.980" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.140" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.010" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="6.510" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved