Premium Feldspar

Alternate Names: Premium Spar

OxideAnalysisFormula
K2O12.12%0.725
Na2O3.03%0.275
Al2O318.18%1.004
SiO266.66%6.248
Oxide Weight563.22
Formula Weight563.22
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Premium Feldspar" descrip="" searchkey="Premium Spar" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="12.120" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.030" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.180" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.660" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved