PotteryCrafts Frit P3195

This is actually Ferro Frit 3195

Alternate Names: PotteryCrafts Frit 3195

OxideAnalysisFormula
CaO11.20%0.674
Na2O5.99%0.326
Al2O312.39%0.410
B2O322.99%1.115
SiO247.44%2.664
Oxide Weight337.58
Formula Weight337.58
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.5
MLRG - Frit Melting Range (C) 920-950C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P3195" descrip="This is actually Ferro Frit 3195" searchkey="PotteryCrafts Frit 3195" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.990" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.390" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="22.990" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="47.440" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved