PotteryCrafts Frit P3124

This is actually Ferro Frit 3124

Alternate Names: PotteryCrafts Frit 3124

OxideAnalysisFormula
CaO14.10%0.697
K2O0.70%0.021
Na2O6.30%0.282
Al2O39.90%0.269
B2O313.70%0.546
SiO255.30%2.553
Oxide Weight277.48
Formula Weight277.48
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.9
MLRG - Frit Melting Range (C) 1000-1020

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P3124" descrip="This is actually Ferro Frit 3124" searchkey="PotteryCrafts Frit 3124" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved