PotteryCrafts Frit P3110

This is actually Ferro Frit 3110

Alternate Names: PotteryCrafts Frit 3110

OxideAnalysisFormula
CaO6.30%0.293
K2O2.30%0.064
Na2O15.30%0.643
Al2O33.70%0.095
B2O32.60%0.097
SiO269.80%3.028
Oxide Weight260.76
Formula Weight260.76
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.1
MLRG - Frit Melting Range (C) 920-950C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P3110" descrip="This is actually Ferro Frit 3110" searchkey="PotteryCrafts Frit 3110" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved