PotteryCrafts Frit P2963

Soft alkaline very high expansion frit

Alternate Names: Potterycrafts Frit 2963

OxideAnalysisFormula
CaO26.50%0.988
MgO0.10%0.005
K2O0.30%0.007
Al2O34.90%0.100
B2O310.80%0.325
SiO252.70%1.834
LOI4.70
Oxide Weight199.36
Formula Weight209.19
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 14.5
MLRG - Frit Melting Range (C) 850-1000C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2963" descrip="Soft alkaline very high expansion frit" searchkey="Potterycrafts Frit 2963" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="26.500" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.900" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="4.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved