PotteryCrafts Frit P2962

High alkaline very high expansion frit

Alternate Names: PotteryCrafts Frit 2962

OxideAnalysisFormula
BaO6.90%0.089
CaO2.90%0.102
K2O10.30%0.216
Na2O18.60%0.593
Al2O35.30%0.103
B2O33.40%0.097
SiO252.50%1.726
Oxide Weight197.41
Formula Weight197.41
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 13.4
MLRG - Frit Melting Range (C) 880-1060C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2962" descrip="High alkaline very high expansion frit" searchkey="PotteryCrafts Frit 2962" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="6.900" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.300" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="18.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved