PotteryCrafts Frit P2961

Standard alkaline frit

Alternate Names: PotteryCrafts Frit 2961

OxideAnalysisFormula
CaO0.20%0.015
MgO0.10%0.010
K2O3.40%0.152
Na2O12.10%0.822
Al2O37.30%0.302
B2O325.20%1.526
SiO250.40%3.534
LOI1.30
Oxide Weight415.93
Formula Weight421.41
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.9
MLRG - Frit Melting Range (C) 900-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2961" descrip="Standard alkaline frit" searchkey="PotteryCrafts Frit 2961" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="25.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.400" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.300" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved