PotteryCrafts Frit P2960

Low Expansion Frit

Alternate Names: PotteryCrafts Frit 2960

OxideAnalysisFormula
CaO3.70%0.332
Li2O1.10%0.186
MgO2.20%0.274
K2O0.20%0.011
ZnO3.20%0.198
Al2O38.50%0.419
B2O317.60%1.271
SiO263.40%5.304
Oxide Weight502.28
Formula Weight502.28
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 3.8
MLRG - Frit Melting Range (C) 1020-1150C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2960" descrip="Low Expansion Frit" searchkey="PotteryCrafts Frit 2960" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.700" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="1.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="3.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved