PotteryCrafts Frit P2959

Low Expansion Frit

Alternate Names: PotteryCrafts Frit 2950

OxideAnalysisFormula
CaO3.69%0.300
MgO2.21%0.250
Na2O5.44%0.400
ZnO0.89%0.050
Al2O36.71%0.300
B2O315.23%0.998
SiO265.84%4.996
Oxide Weight456.06
Formula Weight456.06
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2959" descrip="Low Expansion Frit" searchkey="PotteryCrafts Frit 2950" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.690" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.210" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.440" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="0.890" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.710" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.230" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.840" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved