Potterycrafts Frit P2958

Alternate Names: PotteryCrafts Frit 2958

OxideAnalysisFormula
CaO5.30%0.424
K2O1.34%0.064
Na2O7.08%0.512
Al2O312.07%0.531
B2O316.21%1.045
SiO257.99%4.329
Oxide Weight448.60
Formula Weight448.60
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potterycrafts Frit P2958" descrip="" searchkey="PotteryCrafts Frit 2958" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.340" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="7.080" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.070" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="16.210" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.990" tolerance=""/> </oxides> </material>