PotteryCrafts Frit P2957

Low expansion borax frit

Alternate Names: PotteryCrafts Frit 2957

OxideAnalysisFormula
CaO7.30%0.587
MgO0.20%0.022
K2O2.70%0.129
Na2O3.60%0.262
Al2O39.40%0.415
B2O314.80%0.959
SiO262.00%4.651
Oxide Weight450.83
Formula Weight450.83
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.9
MLRG - Frit Melting Range (C) 1000-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2957" descrip="Low expansion borax frit" searchkey="PotteryCrafts Frit 2957" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="7.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.200" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="62.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved