PotteryCrafts Frit P2955

High alkali low alumina borax frit

Alternate Names: PotteryCrafts Frit 2955

OxideAnalysisFormula
CaO8.80%0.368
K2O8.80%0.219
Na2O10.90%0.413
Al2O39.10%0.209
B2O313.50%0.455
SiO248.90%1.910
Oxide Weight234.69
Formula Weight234.69
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.9
MLRG - Frit Melting Range (C) 920-1050C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2955" descrip="High alkali low alumina borax frit" searchkey="PotteryCrafts Frit 2955" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="8.800" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="8.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved