PotteryCrafts Frit P2953

Borax frit

Alternate Names: PotteryCrafts Frit 2953

OxideAnalysisFormula
CaO14.10%0.607
MgO0.10%0.006
K2O1.70%0.044
Na2O8.80%0.343
Al2O37.50%0.178
B2O318.00%0.625
SiO249.60%1.994
LOI0.20
Oxide Weight241.18
Formula Weight241.66
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.3
MLRG - Frit Melting Range (C) 900-1100C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2953" descrip="Borax frit" searchkey="PotteryCrafts Frit 2953" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.100" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.700" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.500" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved