PotteryCrafts Frit P2952

BORAX FRIT

Alternate Names: PotteryCrafts Frit 2952

OxideAnalysisFormula
CaO4.19%0.437
K2O0.32%0.020
Na2O0.73%0.069
PbO18.09%0.474
Al2O35.29%0.303
B2O315.04%1.263
SiO256.30%5.473
Oxide Weight584.21
Formula Weight584.21
If this formula is not unified correctly please contact us.

No longer available


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2952" descrip="BORAX FRIT" searchkey="PotteryCrafts Frit 2952" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="4.195" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.323" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.737" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="18.097" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.293" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="15.048" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.308" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved