PotteryCrafts Frit P2951

High lead frit

Alternate Names: PotteryCrafts Frit 2951

OxideAnalysisFormula
PbO68.53%1.000
TiO23.07%0.125
SiO228.40%1.539
Oxide Weight325.70
Formula Weight325.70
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="PotteryCrafts Frit P2951" descrip="High lead frit" searchkey="PotteryCrafts Frit 2951" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="68.530" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="3.070" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.400" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved