Alternate Names: 2270 Hvit zircon Boraks fritte, Potclays White Zircon Borax Frit

OxideAnalysisFormula
CaO5.47%0.413
MgO1.06%0.111
Na2O6.06%0.414
ZnO1.17%0.061
Al2O35.68%0.236
B2O313.58%0.827
SiO254.60%3.851
ZrO212.38%0.426
Oxide Weight423.87
Formula Weight423.87
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potclays Frit 2270" descrip="White Zircon Frit" searchkey="2270 Hvit zircon Boraks fritte, Potclays White Zircon Borax Frit" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.470" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.060" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.060" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.170" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.680" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.580" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.600" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="12.380" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved