Potclays Frit 2268

Very high calcium borosilicate frit

Alternate Names: 2268 Kasiumborat fritte, Potclays Calcium Borate Frit

OxideAnalysisFormula
CaO27.10%1.000
Al2O34.78%0.097
B2O350.44%1.500
SiO217.68%0.609
Oxide Weight207.01
Formula Weight207.01
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 950-1050

Discontinued 2007


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potclays Frit 2268" descrip="Very high calcium borosilicate frit" searchkey="2268 Kasiumborat fritte, Potclays Calcium Borate Frit" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="27.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.780" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="50.440" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="17.680" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved