Potclays Frit 2265

Alternate Names: Potclays H.T. Borax Frit

OxideAnalysisFormula
CaO14.68%0.634
MgO0.05%0.003
K2O1.28%0.033
Na2O8.44%0.330
Al2O38.91%0.212
B2O318.09%0.630
SiO248.55%1.958
Oxide Weight242.35
Formula Weight242.35
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potclays Frit 2265" descrip="" searchkey="Potclays H.T. Borax Frit" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.680" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.280" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.440" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.910" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.090" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.550" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved