Potclays Frit 2263

High calcium borosilicate frit

Alternate Names: 2263 Standard boraksfritte, Potclays Standard Borax Frit

OxideAnalysisFormula
CaO15.22%0.634
MgO0.05%0.003
K2O1.33%0.033
Na2O8.75%0.330
Al2O37.55%0.173
B2O318.76%0.630
SiO248.34%1.880
Oxide Weight233.76
Formula Weight233.76
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potclays Frit 2263" descrip="High calcium borosilicate frit" searchkey="2263 Standard boraksfritte, Potclays Standard Borax Frit" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="15.220" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.050" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.330" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.750" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.550" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="18.760" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.340" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved