Potclays Frit 2262

Lead Sesquisilicate Frit

Alternate Names: 2262 Bly halvannensilicat, Potclays Lead Sesquisilicate Frit

OxideAnalysisFormula
PbO68.43%1.000
Al2O33.06%0.098
SiO228.51%1.547
Oxide Weight326.17
Formula Weight326.17
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 880-1080

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potclays Frit 2262" descrip="Lead Sesquisilicate Frit" searchkey="2262 Bly halvannensilicat, Potclays Lead Sesquisilicate Frit" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="68.430" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.510" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved