Potassium Chromate

Formula: K2CrO4

OxideAnalysisFormula
K2O48.50%1.000
Cr2O351.50%0.658
Oxide Weight194.23
Formula Weight194.23
If this formula is not unified correctly please contact us.

A soluble crystalline bright yellow powder. It is used to introduce Chromium oxide into low temperature glazes to achieve colors such as red. The chromium is more effectively dispersed because it is combined with potassium.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potassium Chromate" descrip="" searchkey="" loi="0.00" casnumber="39322-04-8"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="48.500" tolerance=""/> <oxide symbol="Cr2O3" name="Chrome Oxide" status="" percent="51.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved