Potassium Carbonate Trihydrate

Formula: 2K2CO3.3H2O

OxideAnalysisFormula
K2O57.02%1.000
CO226.63
H2O16.34
Oxide Weight94.20
Formula Weight165.18
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Potassium Carbonate Trihydrate" descrip="" searchkey="" loi="0.00" casnumber="584-08-7"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="57.020" tolerance=""/> </oxides> <volatiles> <volatile symbol="CO2" name="Carbon Dioxide" percent="26.630" tolerance=""/> <volatile symbol="H2O" name="Water" percent="16.340" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved