Pot Spar B-801P2

OxideAnalysisFormula
CaO0.01%0.001
MgO0.17%0.024
K2O10.34%0.617
Na2O3.95%0.358
TiO20.01%0.001
Al2O317.58%0.969
SiO265.29%6.107
Fe2O30.07%0.002
LOI0.36
Oxide Weight547.69
Formula Weight549.67
If this formula is not unified correctly please contact us.

A New Zealand material.



By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pot Spar B-801P2" descrip="" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.010" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.170" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.340" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.950" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.010" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.580" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="65.290" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.070" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.360" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved