Podmore Frit P2250

High alkali frit

OxideAnalysisFormula
CaO6.31%0.200
K2O15.90%0.300
Na2O17.44%0.500
Al2O35.74%0.100
B2O33.91%0.100
SiO250.71%1.500
Oxide Weight177.78
Formula Weight177.78
If this formula is not unified correctly please contact us.

Made by Podmore and Sons
Formerly Frit T


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Podmore Frit P2250" descrip="High alkali frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.310" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="15.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="17.440" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.740" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="3.910" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="50.710" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved