Pemco Frit Pb-906

All-fritted opaque glaze

Alternate Names: Frit Pb906

OxideAnalysisFormula
CaO9.57%0.580
K2O2.48%0.090
Na2O1.65%0.091
PbO15.73%0.240
Al2O35.70%0.190
B2O37.36%0.360
SiO249.49%2.801
ZrO28.00%0.221
Oxide Weight340.06
Formula Weight340.06
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.20
GSPT - Frit Softening Point 1550F
MLRG - Frit Melting Range (C) 1500-1670F
IFP - I.F.P. (celsius) 675C

This is Pb-349 wth 8% zirconium silicate. Good base for white and colored opaque glazes. Fires cone 02-6 with 10% clay addition.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-906" descrip="All-fritted opaque glaze" searchkey="Frit Pb906" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.570" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.480" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.650" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="15.730" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.360" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.490" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="8.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved