Pemco Frit Pb-740

High zinc frit for matte glazes cone 06-4

Alternate Names: Frit Pb740

OxideAnalysisFormula
Na2O1.20%0.037
ZnO20.00%0.473
PbO56.80%0.490
Al2O32.00%0.038
SiO220.00%0.641
Oxide Weight192.48
Formula Weight192.48
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.70
GSPT - Frit Softening Point 1600F
MLRG - Frit Melting Range (C) 1560-1650F
IFP - I.F.P. (celsius) 580C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-740" descrip="High zinc frit for matte glazes cone 06-4" searchkey="Frit Pb740" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="20.000" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="56.800" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="20.000" tolerance=""/> </oxides> </material>