Alternate Names: Frit Pb723

OxideAnalysisFormula
Na2O1.50%0.070
PbO71.20%0.930
Al2O32.40%0.069
SiO224.90%1.207
Oxide Weight291.38
Formula Weight291.38
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.00
GSPT - Frit Softening Point 1150F
MLRG - Frit Melting Range (C) 1100-1250F
IFP - I.F.P. (celsius) 490C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-723" descrip="Soda-lead-alumina-silicate low melting glaze frit" searchkey="Frit Pb723" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="71.200" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.400" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="24.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved