Pemco Frit Pb-716

Calcium-lead-silicate frit

Alternate Names: Frit Pb716

OxideAnalysisFormula
CaO5.60%0.248
PbO67.60%0.752
SiO226.80%1.107
Oxide Weight248.33
Formula Weight248.33
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.10
GSPT - Frit Softening Point 1300F
MLRG - Frit Melting Range (C) 1250-1550F
IFP - I.F.P. (celsius) 531C

Used in low tempeature glazes, often with chrome-tin pink and maroon stains.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-716" descrip="Calcium-lead-silicate frit" searchkey="Frit Pb716" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="67.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="26.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved