Pemco Frit Pb-704

Zinc bearing, all-fritted base for cone 1-6

Alternate Names: Frit Pb704

OxideAnalysisFormula
BaO2.60%0.040
CaO9.20%0.391
MgO0.30%0.018
K2O3.50%0.089
Na2O2.10%0.081
ZnO10.60%0.311
PbO6.60%0.071
Al2O35.10%0.119
B2O35.20%0.178
SiO254.30%2.155
ZrO20.50%0.010
Oxide Weight238.54
Formula Weight238.54
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.70
GSPT - Frit Softening Point 1500F
MLRG - Frit Melting Range (C) 1450-1650F
IFP - I.F.P. (celsius) 683C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-704" descrip="Zinc bearing, all-fritted base for cone 1-6" searchkey="Frit Pb704" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.600" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.100" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="6.600" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.300" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="0.500" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved