Pemco Frit Pb-700

Lead alumina bilsilicate frit (1% alumina)

Alternate Names: Frit Pb700

OxideAnalysisFormula
PbO64.99%1.000
Al2O31.01%0.034
SiO234.00%1.943
Oxide Weight343.44
Formula Weight343.44
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.8 x 10-6 (40-450C)
MLRG - Frit Melting Range (C) 1320-1450F
IFP - I.F.P. (celsius) 552C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-700" descrip="Lead alumina bilsilicate frit (1% alumina)" searchkey="Frit Pb700" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="64.990" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.010" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved