Pemco Frit Pb-674

Low expansion (low alkalia) low-lead glaze frit

Alternate Names: Frit Pb674

OxideAnalysisFormula
CaO6.90%0.629
K2O1.10%0.060
Na2O2.80%0.231
PbO3.50%0.080
Al2O35.60%0.281
B2O324.20%1.778
SiO255.90%4.757
Oxide Weight511.47
Formula Weight511.47
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.2 x 10-6 (50-450C)
MLRG - Frit Melting Range (C) 1540-1680F
IFP - I.F.P. (celsius) 645C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-674" descrip="Low expansion (low alkalia) low-lead glaze frit" searchkey="Frit Pb674" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.800" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="3.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.600" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved