Pemco Frit Pb-545

Lead bisilicate

Alternate Names: Frit 545, Frit P545

OxideAnalysisFormula
PbO61.27%1.000
Al2O33.08%0.110
SiO235.64%2.160
Oxide Weight364.24
Formula Weight364.24
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.20
GSPT - Frit Softening Point 1500F
MLRG - Frit Melting Range (C) 1400-1500F
IFP - I.F.P. (celsius) 594C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-545" descrip="Lead bisilicate" searchkey="Frit 545, Frit P545" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="61.279" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.080" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="35.641" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved