1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-316

Alternate Names: Frit P-316, Pemco 316, Pemco Frit Pb316

Oxide Analysis Formula
PbO 61.30% 1.00
Al2O3 7.00% 0.25
SiO2 31.69% 1.92
Oxide Weight 364.07
Formula Weight 364.07

Related Information

Links

Materials Frit
Materials Hommel Frit 4GF79D
Hazards Lead in Frits: The Hazards
Suppliers Pemco International
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit

Data

Co-efficient of Linear Expansion6.0 x 10-6 (50-450C)
Frit Melting Range (C)1400-1550F
I.F.P. (celsius)635C

By Tony Hansen