Pemco Frit Pb-2G30

Low lead calcium frit

Alternate Names: Frit Pb2G30

OxideAnalysisFormula
CaO9.90%0.560
K2O1.60%0.054
Na2O2.50%0.128
PbO18.10%0.258
Al2O36.10%0.190
B2O35.50%0.251
SiO256.30%2.975
Oxide Weight317.59
Formula Weight317.59
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.00
GSPT - Frit Softening Point 1570F
MLRG - Frit Melting Range (C) 1520-1650F
IFP - I.F.P. (celsius) 600C

Dinnerware glaze component - Cone 1 to 4.
Used the same as Pb-349, excellent for underglaze colors.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-2G30" descrip="Low lead calcium frit" searchkey="Frit Pb2G30" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.500" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="18.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved