Pemco Frit Pb-1R99

High expansion lead flux for cone 06 glazes

Alternate Names: Frit Pb1R99

OxideAnalysisFormula
K2O4.40%0.126
Na2O10.90%0.473
PbO33.30%0.401
Al2O37.40%0.195
B2O312.00%0.464
SiO231.90%1.428
Oxide Weight268.76
Formula Weight268.76
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 12.60
GSPT - Frit Softening Point 1170F
MLRG - Frit Melting Range (C) 1150-1200F
IFP - I.F.P. (celsius) 425C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1R99" descrip="High expansion lead flux for cone 06 glazes" searchkey="Frit Pb1R99" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.900" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="33.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.400" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="31.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved