Pemco Frit Pb-1R40

Used in Cone 06 matte glazes

Alternate Names: Frit Pb1R40

OxideAnalysisFormula
BaO15.00%0.254
CaO6.50%0.301
K2O2.20%0.061
Na2O0.60%0.025
PbO30.90%0.359
Al2O33.70%0.094
B2O312.30%0.459
SiO228.80%1.244
Oxide Weight259.62
Formula Weight259.62
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.60
GSPT - Frit Softening Point 1420F
MLRG - Frit Melting Range (C) 1380-1500F
IFP - I.F.P. (celsius) 580C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1R40" descrip="Used in Cone 06 matte glazes" searchkey="Frit Pb1R40" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="15.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved