Pemco Frit Pb-1N84

Very low melting high lead borosilicate

Alternate Names: Frit Pb1N84

OxideAnalysisFormula
PbO83.00%1.000
B2O310.00%0.386
SiO27.00%0.313
Oxide Weight268.92
Formula Weight268.92
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.10
GSPT - Frit Softening Point 860F
MLRG - Frit Melting Range (C) 840-890F
IFP - I.F.P. (celsius) 375C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1N84" descrip="Very low melting high lead borosilicate" searchkey="Frit Pb1N84" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="83.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="7.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved