Pemco Frit Pb-1M90

Titanium bearing matte glaze component at Cone 01

Alternate Names: Frit Pb1M90

OxideAnalysisFormula
CaO3.60%0.222
K2O4.60%0.169
Na2O3.40%0.190
PbO27.10%0.420
TiO27.70%0.333
Al2O37.80%0.264
B2O39.70%0.482
SiO236.10%2.077
Oxide Weight345.71
Formula Weight345.71
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.50
GSPT - Frit Softening Point 1700F
MLRG - Frit Melting Range (C) 1650-1750F
IFP - I.F.P. (celsius) 550C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1M90" descrip="Titanium bearing matte glaze component at Cone 01" searchkey="Frit Pb1M90" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.600" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.400" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="27.100" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="7.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="9.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.100" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved