Pemco Frit Pb-1K75

Cone 06 all-fritted transparent gloss glaze

Alternate Names: Frit Pb1K75

OxideAnalysisFormula
CaO5.50%0.357
K2O1.90%0.073
Na2O1.80%0.106
F3.60%0.690
PbO28.40%0.464
Al2O33.80%0.136
B2O313.00%0.680
SiO240.80%2.473
ZrO21.20%0.035
Oxide Weight364.32
Formula Weight364.32
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.30
GSPT - Frit Softening Point 1370F
MLRG - Frit Melting Range (C) 1320-1420F
IFP - I.F.P. (celsius) 505C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1K75" descrip="Cone 06 all-fritted transparent gloss glaze" searchkey="Frit Pb1K75" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.500" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.900" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.800" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="3.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="28.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.800" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="1.200" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved