Pemco Frit Pb-1325

High lead borosilicate with small amount of sodium

Alternate Names: Frit Pb1325

OxideAnalysisFormula
Na2O2.90%0.204
PbO40.80%0.796
B2O335.70%2.234
SiO220.60%1.493
Oxide Weight435.60
Formula Weight435.60
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.3 x 10-6 (50-450C)
GSPT - Frit Softening Point 1260F
MLRG - Frit Melting Range (C) 1260-1330F
IFP - I.F.P. (celsius) 490C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1325" descrip="High lead borosilicate with small amount of sodium" searchkey="Frit Pb1325" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.900" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="40.800" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="35.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="20.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved