Pemco Frit Pb-1307

High lead zinc containing wall tile frit

Alternate Names: Frit Pb1307

OxideAnalysisFormula
CaO5.40%0.231
Na2O2.20%0.085
ZnO8.70%0.256
PbO39.90%0.428
Al2O36.30%0.148
B2O39.20%0.317
SiO228.30%1.128
Oxide Weight239.59
Formula Weight239.59
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.8 x 10-6 (50-450C)
GSPT - Frit Softening Point 1250F
MLRG - Frit Melting Range (C) 1250-1300F
IFP - I.F.P. (celsius) 547C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1307" descrip="High lead zinc containing wall tile frit" searchkey="Frit Pb1307" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="5.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="8.700" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="39.900" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="6.300" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="9.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="28.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved