Pemco Frit Pb-1279

Very low lead barium frit for partially fritted glazes cone 04-5

Alternate Names: Frit Pb1279

OxideAnalysisFormula
BaO4.10%0.063
CaO6.90%0.288
MgO2.00%0.116
K2O3.50%0.087
Na2O5.10%0.192
ZnO7.60%0.218
PbO3.40%0.036
Al2O312.70%0.291
B2O32.10%0.071
SiO252.60%2.048
Oxide Weight233.98
Formula Weight233.98
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.5 x 10-6 (50-450C)
GSPT - Frit Softening Point 1600F
MLRG - Frit Melting Range (C) 1550-1940F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1279" descrip="Very low lead barium frit for partially fritted glazes cone 04-5" searchkey="Frit Pb1279" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="4.100" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.900" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.000" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.500" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.100" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="7.600" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="3.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.700" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved