Pemco Frit Pb-1241

Leaded sodium and potassiun free frit

Alternate Names: Frit Pb1241

OxideAnalysisFormula
CaO10.40%0.480
MgO0.30%0.019
PbO43.10%0.500
Al2O34.00%0.102
B2O35.90%0.220
SiO236.30%1.565
Oxide Weight259.12
Formula Weight259.12
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.9 x 10-6 (50-450C)
GSPT - Frit Softening Point 1400F
MLRG - Frit Melting Range (C) 1380-1510F
IFP - I.F.P. (celsius) 625C

All fritted base for Cone 05 through Cone 1 with 10% clay addition.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1241" descrip="Leaded sodium and potassiun free frit" searchkey="Frit Pb1241" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.400" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.300" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="43.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="5.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="36.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved