Pemco Frit Pb-1151

Leaded titanium frit

Alternate Names: Frit Pb1151

OxideAnalysisFormula
CaO3.30%0.206
K2O4.10%0.152
Na2O2.80%0.158
F1.30%0.240
PbO30.80%0.483
TiO29.00%0.395
B2O36.10%0.307
SiO243.90%2.558
Oxide Weight354.81
Formula Weight354.81
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 9.5 x 10-6 (50-450C)
GSPT - Frit Softening Point 1400F
MLRG - Frit Melting Range (C) 1350-1450F
IFP - I.F.P. (celsius) 685C

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Pemco Frit Pb-1151" descrip="Leaded titanium frit" searchkey="Frit Pb1151" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="3.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.800" tolerance=""/> <oxide symbol="F" name="Fluorine" status="" percent="1.300" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="30.800" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="9.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="43.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved